Esmael Rostami, Abdolkarim Zare, Masume Zangooei


Newpolyamides containing á,áï‚¢-Xylyldithiophenoxide Unitswere prepared under microwave irradiation and their solubility, thermal behavior, viscosities and nanostructures were evaluated. These polyamides showed good solubility in a series of organic solvents. The viscosities of these polyamides are in the range of 0.41-0.54 dl/g. Glass transition temperatures are in the range of 214-251°C. Temperatures for 10% weight loss (T10) are in the range of 286-323°C, temperatures for 50% weight loss (T50) are in the range of 463-535°C and char yields are in the range of 21-41%; and these results shows the thermal stabilities of the prepared polyamides. Supramolecular assemblies showed nanostructures.


Haftungsausschluss: Dieser Abstract wurde mit Hilfe von Künstlicher Intelligenz übersetzt und wurde noch nicht überprüft oder verifiziert

Indiziert in

  • CASS
  • Google Scholar
  • Öffnen Sie das J-Tor
  • Nationale Wissensinfrastruktur Chinas (CNKI)
  • CiteFactor
  • Kosmos IF
  • Verzeichnis der Indexierung von Forschungszeitschriften (DRJI)
  • Geheime Suchmaschinenlabore
  • Impact Factor für wissenschaftliche Artikel (SAJI)
  • ICMJE

Mehr sehen

Flyer